Thermal Properties of ZrB₂-TiB₂ Solid Solutions

Research output: Contribution to journal › Article › peer-review

Abstract

Zirconium diboride ceramics were prepared with additions of up to 50 vol.% TiB 2 . The resulting (Zr,Ti)B 2 ceramics formed complete solid solutions based on x-ray diffraction. The addition of TiB 2 resulted in grain size decreasing from 22 μm for nominally pure ZrB 2 to 7 μm for ZrB 2 -50 vol.% TiB 2 . The thermal conductivity at 25°C ranged from 93 W/m⋅K for nominally pure ZrB 2 to 58 W/m⋅K for ZrB 2 -50 vol.% TiB 2 . Thermal conductivity was as high as 67 W/m⋅K for nominally pure ZrB 2 at 2000°C, but dropped to 59 W/m K with the addition of 50 vol.% TiB 2 . Electrical resistivity measurements were used to calculate the electron contribution to thermal conductivity, which was 76 W/m⋅K for nominally pure ZrB 2 decreasing to 57 W/m⋅K when 50 vol.% TiB 2 was added. The phonon contribution to thermal conductivity did not change significantly for ≤ 10 vol.% TiB 2 . Additions of ≥ 25 vol.% TiB 2 reduced the phonon contribution to nearly zero for all temperatures.

Original languageAmerican English
Pages (from-to)7434-7441
Number of pages8
JournalJournal of the European Ceramic Society
Volume41
Issue number15
DOIs
StatePublished - Dec 1 2021

Keywords

  • Solid Solution
  • Thermal Conductivity
  • Titanium Diboride
  • Zirconium Diboride

Disciplines

  • Ceramic Materials

Fingerprint

Dive into the research topics of 'Thermal Properties of ZrB₂-TiB₂ Solid Solutions'. Together they form a unique fingerprint.

Cite this