Tantalum diboride (TaB2) was synthesized by reducing Ta2O5 using B4C and graphite at 1600 °C under flowing Ar. The powder had an average particle size of 0.4 μm with both needle-like and rounded particles. The TaB2 powder was hot pressed to relative densities of 97% at 2000 °C (3.6 μm grain size) and 98% at 2100 °C (5.3 μm grain size). Mechanical properties were measured for TaB2 hot pressed at 2100 °C and were comparable to those of the commonly studied diborides, ZrB2 and HfB2. The Young's modulus was 551 GPa, Vickers' hardness was 25.6 GPa, flexure strength was 555 MPa, and fracture toughness was 4.5 MPa-m1/2.

Original languageAmerican English
Pages (from-to)4251-4253
Number of pages3
JournalMaterials Letters
Volume62
Issue number27
DOIs
StatePublished - Jun 1 2008

Keywords

  • Hot Pressing
  • Mechanical Properties
  • Synthesis
  • Tantalum Diboride (TaB2)

Disciplines

  • Materials Science and Engineering

Fingerprint

Dive into the research topics of 'Synthesis, Densification, and Mechanical Properties of TaB₂'. Together they form a unique fingerprint.

Cite this