SiC Platelet Reinforced Al₂O₃ Composites by Free Sintering of Coated Powders

Research output: Contribution to journal › Article › peer-review

Abstract

SiC platelets were coated with the required thickness of fine-grained Al2O3 powder by controlled heterogeneous precipitation from a solution. after calcination, the coated platelets were compacted and sintered at a constant heating rate of 5 °C/min in a helium atmosphere. the parameters which control the coating process and the sintering behavior of the coated platelets are outlined. Starting with an initial matrix density of 40-45% of the theoretical, composites containing ≈20 vol% platelets reached nearly full density after sintering at 1800 °C for 30 minutes. by comparison, similar composites formed by mechanical mixing of the SiC platelets and the precipitated Al2O3 powder reached a density of only ≈70 % of the theoretical under identical sintering conditions.

Original languageAmerican English
JournalCeramic Engineering and Science Proceedings
DOIs
StatePublished - Jan 1 1994

Keywords

  • Calcination
  • Coated Platelets
  • Constant Heating Rate
  • Controlled Heterogeneous Precipitation
  • SiC Platelets

Disciplines

  • Materials Science and Engineering

Fingerprint

Dive into the research topics of 'SiC Platelet Reinforced Al₂O₃ Composites by Free Sintering of Coated Powders'. Together they form a unique fingerprint.

Cite this