Skip to main navigation Skip to search Skip to main content

Processing and Room Temperature Mechanical Properties of a Zirconium Carbide Ceramic

Research output: Contribution to journal › Article › peer-review

Abstract

Zirconium carbide (ZrC) powder, batched to a ratio of 0.98 C/Zr, was prepared by carbothermal reduction of ZrO 2 with carbon black. Nominally phase-pure ZrC powder had a mean particle size of 2.4 μm. The synthesized powder was hot-pressed at 2150°C to a relative density of > 95%. The mean grain size was 2.7 ± 1.4 μm with a maximum observed grain size of 17.5 μm. The final hot-pressed billets had a C/Zr ratio of 0.92, and oxygen content of 0.5 wt%, as determined by gas fusion analysis. The mechanical properties of ZrC 0.92 O 0.03 were measured at room temperature. Vickers’ hardness decreased from 19.5 GPa at a load of 0.5 kgf to 17.0 GPa at a load of 1 kgf. Flexural strength was 362.3 ± 46 MPa, Young's modulus was 397 ± 13 MPa, and fracture toughness was 2.9 ± 0.1 MPa•m 1/2 . Analysis of mechanical behavior revealed that the largest ZrC grains were the strength-limiting flaw in these ceramics.

Original languageAmerican English
Pages (from-to)413-418
Number of pages6
JournalJournal of the American Ceramic Society
Volume104
Issue number1
DOIs
StatePublished - Jan 1 2021

Keywords

  • Characterization
  • Mechanical Properties
  • Processing

Disciplines

  • Ceramic Materials

Fingerprint

Dive into the research topics of 'Processing and Room Temperature Mechanical Properties of a Zirconium Carbide Ceramic'. Together they form a unique fingerprint.

Cite this