Abstract
The synergistic roles of boron carbide and carbon additions in the enhanced densification of zirconium diboride (ZrB2) by pressureless sintering have been studied. ZrB2 was sintered to >99% relative density at 1900°C. the combination of 2 wt% boron carbide and 1 wt% carbon promoted densification by removing surface oxide impurities (ZrO2 and B2O3) and inhibiting grain growth. Four-point bending strength (473±43 MPa), Vickers' microhardness (19.6±0.4 GPa), fracture toughness (3.5±0.6 MPa·m1/2), and Young's modulus (507 GPa) were measured. Thermal gravimetry showed that the combination of additives did not have an adverse effect on the oxidation behavior.
| Original language | American English |
|---|---|
| Journal | Journal of the American Ceramic Society |
| DOIs | |
| State | Published - Nov 1 2007 |
Keywords
- Carbon Additions
- Pressureless Densification
- Zirconium Diboride
Disciplines
- Materials Science and Engineering
Fingerprint
Dive into the research topics of 'Pressureless Densification of Zirconium Diboride with Carbon Additions'. Together they form a unique fingerprint.Cite this
- APA
- Standard
- Harvard
- Vancouver
- Author
- BIBTEX
- RIS