Abstract

The oxidation resistance of zirconium diboride (ZrB2) ceramics with tungsten carbide (WC) additions was studied. ZrB2 ceramics, nominally pure and with WC additions of 4, 5, and 6 mol%, were densified by pressureless sintering. During heating, the WC that was added to the ceramic dissolved into the ZrB2 matrix, forming a solid solution. Oxidation behavior was evaluated using isothermal furnace oxidation at 1500°C and 1600°C. the presence of tungsten reduced both the weight gain and oxide scale thickness compared with nominally pure ZrB2. after oxidation at 1600°C for 3 h, the thickness of the ZrO2 outer scale was reduced from 4.7 mm for nominally pure ZrB2 to 0.5 mm for the ceramic containing 6 mol% WC. Analysis showed that WC additions improved the oxidation resistance of ZrB2 by changing the morphology of the zirconia scale formed during oxidation.

Original languageAmerican English
Pages (from-to)1198-1205
Number of pages8
JournalJournal of the American Ceramic Society
Volume94
Issue number4
DOIs
StatePublished - Apr 1 2011

Disciplines

  • Materials Science and Engineering

Fingerprint

Dive into the research topics of 'Oxidation of Zirconium Diboride with Tungsten Carbide Additions'. Together they form a unique fingerprint.

Cite this