Microstructure and Mechanical Properties of Reaction-Hot-Pressed Zirconium Diboride based Ceramics

  • Missouri University of Science and Technology

Research output: Contribution to journal › Article › peer-review

Abstract

ZrB 2 ceramics were prepared by in-situ reaction hot pressing of ZrH 2 and B. Additions of carbon and excess boron were used to react with and remove the residual oxygen present in the starting powders. Additions of tungsten were utilized to make a ZrB 2 -4 mol%W ceramic, while a change in the B/C ratio was used to produce a ZrB 2 -10 vol% ZrC ceramic. All three compositions reached near full density. The baseline ZrB 2 and ZrB 2 -ZrC composition contained a residual oxide phase and ZrC inclusions, while the W-doped composition contained residual carbon and a phase that contained tungsten and boron. All three compositions exhibited similar values for flexure strength (~520 MPa), Vickers hardness (~15 GPa), and elastic modulus (~500 to 540 GPa). Fracture toughness was about 2.6 MPa · m 1/2 for the W-doped ZrB 2 compared to about 3.8 MPa · m 1/2 for the ZrB 2 and ZrB 2 -ZrC ceramics. This decrease in fracture toughness was accompanied by an observed absence of crack deflection in the W-doped ZrB 2 compared with the other compositions. The study demonstrated that reaction-hot-pressing can be used to fabricate ZrB 2 based ceramics containing solid solution additives or second phases with comparable mechanical properties.

Original languageAmerican English
JournalInternational Journal of Applied Ceramic Technology
Volume16
DOIs
StatePublished - Apr 1 2019

Keywords

  • Mechanical Properties
  • Reactive Hot-Pressing
  • Tungsten
  • UHTC
  • Zirconium Carbide
  • Zirconium Diboride