Abstract
<p> The microstructural evolution and grain-boundary influence on electrical properties of Ce0.90Gd0.10O1.95 were studied. the nanoscale powders synthesized from a semibatch reactor exhibited 50% green density and 92% sintering density at 1200°C (∼200°C lower than previous studies). Impedance spectra as a function of temperature and grain size were analyzed. the Ce0.90Gd0.10O1.95 with finest grain size possessed highest overall grain-boundary resistance; this contribution was eliminated at temperatures >600°C, regardless of grain size. the grain conductivity was independent of grain size and was dependent on temperature with two distinct regimes, indicative of the presence of Gd′Ce−Vo∘∘ complexes that dissociated at a critical temperature of ∼580°C. the activation energy for complex dissociation was ∼0.1 eV; the value for the grain-boundary was ∼1.2eV, which was size independent.</p>
| Original language | American English |
|---|---|
| Pages (from-to) | 1757-1762 |
| Number of pages | 6 |
| Journal | Journal of the American Ceramic Society |
| Volume | 85 |
| Issue number | 7 |
| DOIs | |
| State | Published - Dec 1 2004 |
Keywords
- Cerium/Cerium Compounds
- Grain Boundaries
- Conductivity
- Microstructure
Disciplines
- Materials Science and Engineering
Fingerprint
Dive into the research topics of 'Microstructure and Grain-boundary Effect on Electrical Properties of Gadolinium-doped Ceria'. Together they form a unique fingerprint.Cite this
- APA
- Standard
- Harvard
- Vancouver
- Author
- BIBTEX
- RIS