Skip to main navigation Skip to search Skip to main content

Fabrication and Properties of Reactively Hot Pressed ZrB₂-SiC Ceramics

Research output: Contribution to journal › Article › peer-review

Abstract

ZrB 2 -SiC ceramics with relative densities >99% were fabricated by 'in situ' reactive hot pressing from ZrH 2 , B 4 C and Si. the reaction was studied using two processes, (1) powder reactions at temperatures from 1150 to 1400 °C and (2) reactive hot pressing between 1600 and 1900 °C. the products from the reaction of a 2ZrH 2 :1B 4 C:1Si molar mixture were ZrB 2 , SiC, ZrO 2 and ZrC. Modification of the composition to 2ZrH 2 :1.07B 4 C:1.16Si resulted in the elimination of the undesired ZrO 2 and ZrC phases. the final composition was approximately ZrB 2 -27 vol% SiC with no undesired phases detected by X-ray diffraction, and only low concentrations of B 4 C detected by scanning electron microscopy. Elimination of the undesired phases was accomplished by removing surface oxides through chemical reactions at elevated temperatures. Reactively hot pressed samples consisting of ZrB 2 with 27 vol% SiC had a Young's modulus of 508 GPa, a flexure strength of 720 MPa, a fracture toughness of 3.5 MPa m 1/2 and a Vickers' hardness of 22.8 GPa.

Original languageAmerican English
Pages (from-to)2729-2736
Number of pages8
JournalJournal of the European Ceramic Society
Volume27
Issue number7
DOIs
StatePublished - Jan 1 2007

Keywords

  • Borides
  • Mechanical Properties
  • Microstructure-Final
  • Reactive Hot Pressing
  • SiC

Disciplines

  • Materials Science and Engineering

Fingerprint

Dive into the research topics of 'Fabrication and Properties of Reactively Hot Pressed ZrB₂-SiC Ceramics'. Together they form a unique fingerprint.

Cite this