Skip to main navigation Skip to search Skip to main content

Effect of ZrB₂ Content on the Densification, Microstructure, and Mechanical Properties of ZrC-SiC Ceramics

Research output: Contribution to journal › Article › peer-review

Abstract

ZrC ceramics containing 30 vol% SiC-ZrB 2 were produced by high-energy ball milling and reactive hot pressing. The effects of ZrB 2 content on the densification, microstructure, and mechanical properties of ceramics were investigated. Fully dense ceramics were achieved as ZrB 2 content increased to 10 and 15 vol%. The addition of ZrB 2 suppressed grain growth and promoted dispersion of the SiC particles, resulting in fine and homogeneous microstructures. Vickers hardness increased from 23.0 ± 0.5 GPa to 23.9 ± 0.5 GPa and Young's modulus increased from 430 ± 3 GPa to 455 ± 3 GPa as ZrB 2 content increased from 0 to 15 vol%. The increases were attributed to a combination of the higher relative density of ceramics with higher ZrB 2 content and the higher Young's modulus and hardness of ZrB 2 compared to ZrC. Indentation fracture toughness increased from 2.6 ± 0.2 MPa·m 1/2 to 3.3 ± 0.1 MPa·m 1/2 as ZrB 2 content increased from 0 to 15 vol% due to the increase in crack deflection by the uniformly dispersed SiC particles. Compared to binary ZrC-SiC ceramics, ternary ZrC-SiC-ZrB 2 ceramics with finer microstructure and higher relative densities were achieved by the addition of ZrB 2 particles.

Original languageAmerican English
Pages (from-to)220-225
Number of pages6
JournalJournal of the European Ceramic Society
Volume40
Issue number2
DOIs
StatePublished - Feb 1 2020

Keywords

  • Densification
  • Mechanical Properties
  • Microstructure
  • Reactive Hot Pressing
  • Zirconium Carbide-Silicon Carbide-Zirconium Diboride

Disciplines

  • Ceramic Materials

Fingerprint

Dive into the research topics of 'Effect of ZrB₂ Content on the Densification, Microstructure, and Mechanical Properties of ZrC-SiC Ceramics'. Together they form a unique fingerprint.

Cite this