Atomic Layer Deposition of Hafnium(IV) Oxide on Graphene Oxide: Probing Interfacial Chemistry and Nucleation by using X-ray Absorption and Photoelectron Spectroscopies

  • Theodore E.G. Alivio
  • , Luis R. De Jesus
  • , Robert V. Dennis
  • , Ye Jia
  • , Cherno Jaye
  • , Daniel A. Fischer
  • , Uttam Singisetti
  • , Sarbajit Banerjee
  • Texas A&M University
  • Dept. of Industrial Engineering University at Buffalo
  • National Institute of Standards and Technology

Research output: Contribution to journal › Article › peer-review

Original languageEnglish
Pages (from-to)2842-2848
Number of pages7
JournalChemPhysChem
Volume16
Issue number13
DOIs
StatePublished - Sep 1 2015
Externally publishedYes

ASJC Scopus Subject Areas

  • Atomic and Molecular Physics, and Optics
  • Physical and Theoretical Chemistry

Keywords

  • atomic layer deposition
  • graphene oxide
  • hafnium(IV) oxide
  • NEXAFS
  • XPS

Fingerprint

Dive into the research topics of 'Atomic Layer Deposition of Hafnium(IV) Oxide on Graphene Oxide: Probing Interfacial Chemistry and Nucleation by using X-ray Absorption and Photoelectron Spectroscopies'. Together they form a unique fingerprint.

Cite this